Entec Hypro™ PPC-GF20 Natural Impact Polypropylene, 20% Glass Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Entec Engineered Resins
Trade Name Hypro™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypro™ PPC-GF20 Natural Impact Polypropylene, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Entec
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 10.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.9 MPa
8110 psi
ASTM D638
Elongation at Break 5.00 %
5.00 %
ASTM D638
Elongation at Yield 4.00 %
4.00 %
ASTM D638
Flexural Strength 64.0 MPa
9280 psi
ASTM D790
Flexural Modulus 2.897 GPa
420.2 ksi
tangent; ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
289 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648