Material Notes:
EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and gloss.Applications: EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and glossInformation provided by Equate
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D792
Melt Flow 20 g/10 min

@Load 2.16 kg
20 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength at Break 21.0 MPa
3050 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Modulus 1.15 GPa
167 ksi
ASTM D790
Izod Impact, Unnotched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Middle Barrel Temperature 175 - 245 °C
347 - 473 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F