Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 43
43
ASTM D2240
Tensile Strength, Yield 10.3 MPa
1500 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 0.121 GPa
17.5 ksi
1% Secant; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
Rate A, Loading 1 (10 N); ASTM D1525