Material Notes:
TECAST VEKTON™ 6PB cushion pads are used to dampen the shock load on the anvil of a pile hammer. Specially formulated from an impact-modified type 6 nylon, they combine the excellent strength of nylon with the impact-resistance of the modifier. TECAST VEKTON™ 6PB cushion pads are brilliant OSHA orange to provide easy identification.Excellent shock load characteristics protect expensive hammer anvilsHigh energy transmittance effectively uses hammer force to drive pileInformation Provided by Ensinger Industries, Inc.
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110 - 115
110 - 115
Tensile Strength, Yield 64.1 - 73.1 MPa

@Temperature 22.8 °C
9300 - 10600 psi

@Temperature 73.0 °F
Modulus of Elasticity 2.55 - 2.93 GPa

@Temperature 22.8 °C
370 - 425 ksi

@Temperature 73.0 °F
Compressive Strength 79.3 - 89.6 MPa

@Temperature 22.8 °C
11500 - 13000 psi

@Temperature 73.0 °F
at 1% Deformation
Shear Strength 44.8 - 51.7 MPa

@Temperature 22.8 °C
6500 - 7500 psi

@Temperature 73.0 °F
Izod Impact, Notched 0.427 - 0.534 J/cm

@Temperature 22.8 °C
0.800 - 1.00 ft-lb/in

@Temperature 73.0 °F