Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)

Category Polymer , Thermoplastic , Polyimide, Thermoplastic , Thermoplastic Polyimide, Graphite Filled , Thermoplastic Polyimide, Molded, PTFE Filled
Manufacturer Ensinger
Trade Name TECASINT
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.Main FeaturesHigh thermal and mechanical capacityGood radiation-resistanceLow outgassingEasily machined to tight tolerancesFlame retardant according to UL94 V-0Very creep resistantGood sliding propertiesBroad chemical compatibilitySensitive to hydrolysis in higher thermal rangeApplicationsMechanical engineeringMaterials handling equipmentAircraft and aerospace industriesPrecision engineeringAutomotive industryNuclear and vacuum technologyTextile industryPreferred FieldsValve seating, switch parts, chain guides, piston rings, guide piece, thrust washer, bearingsInformation Provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.48 g/cc

@Temperature 23.0 °C
0.0535 lb/in³

@Temperature 73.4 °F
DIN 53 479
Filler Content 10 %
10 %
PTFE
15 %
15 %
Graphite
Water Absorption 2.3 %

@Temperature 80.0 °C
2.3 %

@Temperature 176 °F
3 week saturation; EN ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 85

@Temperature 23.0 °C
85

@Temperature 73.4 °F
DIN 53 505
Tensile Strength, Yield 77.0 MPa

@Temperature 23.0 °C
11200 psi

@Temperature 73.4 °F
EN ISO 527
Elongation at Break 2.9 %

@Temperature 23.0 °C
2.9 %

@Temperature 73.4 °F
EN ISO 527
Elongation at Yield 3.6 %
3.6 %
Flexural; EN ISO 178
Flexural Strength 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
EN ISO 178
Compressive Yield Strength 227 MPa
32900 psi
10% Strain; EN ISO 604
Compressive Strength 227 MPa

@Temperature 23.0 °C
32900 psi

@Temperature 73.4 °F
EN ISO 604
Izod Impact, Notched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 51.0 µm/m-°C

@Temperature 50.0 - 200 °C
28.3 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Glass Transition Temp, Tg 330 °C
626 °F
DMTA
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Color Black Gleamy
DIN-Abbreviation PI CS15 TF10