Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer Ensinger
Trade Name HYDEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger HYDEX® 4101L Polybutylene Terephthalate (PBT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HYDEX® 4101 & 4101L (lubricated) is a very stable chemical compound that can withstand high impact without deterioration. It is approved for direct contact with food by the FDA and is ideal for machined parts in food processing equipment. HYDEX® 4101 has excellent resistance to typical cleaning chemicals such as chlorine and caustic solutions and has a very low moisture absorption rate, as much as 15 times less than nylon.Good chemical resistance propertiesHigh impact strengthFDA approved for use in food processingA wear factor up to 50% better than PET-PVery low moisture absorption rateExcellent machining qualitiesNo center line porosityHYDEX® 4101 & 4101L exhibits a broad range of outstanding properties for a variety of applications, especially in the food processing industry. It is ideal for applications such as cams, bearings, gears, food pistons, wear strips, scraper blades, valve bodies and conveyor components.Information Provided by Ensinger Industries, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 49.6 MPa
7200 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Tensile Modulus 2.62 GPa
380 ksi
ASTM D638
Flexural Modulus 2.69 GPa

@Temperature 22.8 °C
390 ksi

@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.11
0.11
vs Steel; LNP EPALP-TB001
Coefficient of Friction, Static 0.080
0.080
Steel; LNP EPALP-TB001
K Factor (Wear Factor) 38
38
in<sup>5</sup>-min/ft-lbs/hr, at 2000 PV; LNP EPALP-TB001
Limiting Pressure Velocity 0.550 MPa-m/sec
15700 psi-ft/min
LNP EPALP-TB003, at 100 ft/min
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
UL746B
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C
195 °F
ASTM D648
Descriptive Properties Value Comments
3A Compliant YES
FDA Complaint YES
USDA Compliant YES
Users viewing this material also viewed the following: