Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Engineered Polymer Solutions PET 5300 FR, 30% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer Engineered Polymer Solutions
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Engineered Polymer Solutions PET 5300 FR, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural and colors available. Injection molding grade. Uses: General Purpose, pump housings, electricalInformation provided by Engineered Polymer Solutions.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 124 MPa
18000 psi
ASTM D638
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 221 °C
430 °F
ASTM D648
Flammability, UL94 V-0
V-0
0.0625 in.