Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 31.7 MPa @Thickness 3.20 mm |
4600 psi @Thickness 0.126 in |
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 5112 C Clarified Random Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 31.7 MPa @Thickness 3.20 mm |
4600 psi @Thickness 0.126 in |
At 51mm/min, thick injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 5135 C Clarified Polypropylene Random Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ 34-1520 Silver Metallic TFPP Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | Type 1 Specimen, Rate: 2"/min; ASTM D638 |
Global PP-100 General Purpose Polypropylene Homopolymer, Controlled Rheology Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
LyondellBasell Petrothene® LM600700 High Density Polyethylene (Blow Molding Grade) ApplicationsPETROTHENE LM 6007-00 resin exhibits very low taste and odor characteristics as well as good rigidity. Typical applications include water, and milk and juice bottles.Regulatory StatusLM.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Ineos R12C-01 Polypropylene Random Copolymer Grade R12C-01 is a high clarity, antistatic polypropylene copolymer for injection molding and stretch blow molding applications. This material meets the requirements of the U.S. Food and Drug Admini.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Spartech Royalite R87/59 ABS/PVC Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Techmer ES HiFill® PP GF/M30 CC BK 30% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 30% Filler by WeightFeatures: Chemically Coupled and CopolymerAppearance: BlackInformation provided by TP Composites, In.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Techmer ES Luriblend® ABS SL2 Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive Ablebond 724-1 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates.Information provided by Tra-Con Inc. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR N330 (HAF) Black MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | 2 in/min; ASTM D638 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite 350A0096914 Propionate Natural Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite 360E3V45512 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers Centrex® 833 Sheet Extrusion Grade Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Dow 5E16S Polypropylene Homopolymer Resin OverviewConsistent processabilitySuperior impactGood mold releaseContains an antistatic additiveComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aComplies with Canadian HPFB No ObjectionDOW 5E16S Polypr.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Entec Hypel® PEHD.7/.962 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | D638 |
Ineos H03W-00 Polypropylene Homopolymer Grade H03W-00 is a homopolymer designed for extrusion processing. It exhibits low water carry over. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 C.. |
|||
Tensile Strength, Yield | 31.7 MPa | 4600 psi | ASTM D638 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |