Eliokem Chemigum® P86F Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eliokem
Trade Name Chemigum®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eliokem Chemigum® P86F Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fine particle size. 33% bound ACN. Crosslinked polymer structure. CaCO3 partitioning agent.Can be used in TPU and phenolic blends.Used in friction materials such as disc-pads and brake linings.Information provided by Eliokem.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Particle Size 400 µm
400 µm
Median
Mooney Viscosity 55

@Temperature 100 °C
55

@Temperature 212 °F
ML 1+4