Solvay RHODOPOL® 23 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOPOL® 23 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rhodopol® 23 is Standard grade Xanthan Gum. It exhibits high pseudoplastic behavior and rapid hydration rate. This grade is registered on the FALCON list of approved substances.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available in: Asia Pacific, Europe, Latin America and North America.Applications: Painting, Agrochemical, Detergency, Pottery industry and Public worksInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.750 g/cc
0.0271 lb/in³
Loss On Ignition <= 13 %
<= 13 %
TI-0515
Particle Size >= 300 µm
>= 300 µm
<2%, 50 Mesh; TI-2087
pH 6.0 - 8.0
6.0 - 8.0
1% aq. Sol.; TI-2076
Brookfield Viscosity 200 - 1800 cP
200 - 1800 cP
1% sol. in 1% KCl Brookfield LV 60 rpm spindle n°3; TI-1110
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Fine Powder
Color Cream
Loss on drying <13%
TI-0515