Elastocon TPE Technologies Elastocon® STK56PA-B Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Elastocon TPE Technologies
Trade Name Elastocon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Elastocon TPE Technologies Elastocon® STK56PA-B Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elastocon® STK56PA-B black thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA-B is well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics, sound and vibration dampening, improved impact resistance, and U.V. stability. Elastocon® STK56PA-B can be overmolded to nylon.Information provided by Elastocon TPE Technologies, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.025 cm/cm
0.015 - 0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength 5.60 MPa
812 psi
ASTM D412
Elongation at Break 192 %
192 %
ASTM D412
100% Modulus 0.00420 GPa
0.609 ksi
ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 249 - 260 °C
480 - 500 °F
Front Barrel Temperature 266 - 277 °C
510 - 530 °F
Nozzle Temperature 277 - 285 °C
530 - 545 °F
Mold Temperature 82.2 - 104 °C
180 - 220 °F
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Descriptive Properties Value Comments
Injection Rate Fast