Material Notes:
Low-density polyethylene 1924P is a resin in the boardstock coating industry for use in breadboard, cupstock, and liquid packaging board. This material has an excellent combination of low neck-in, ease of processing, good chill-roll release, low coefficient of friction (for ease of indexing carton blanks) and good heat sealability. It is characterized by high-speed processability, excellent drawdown and reliable lot-to-lot consistency.List of Applications:Food-contact applicationsPhotographic paperInformation supplied by the manufacturer.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D4883
Melt Flow 4.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.0 MPa
1450 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Tensile Strength, Yield 14.0 MPa
2030 psi
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Elongation at Break 100 %
100 %
500 mm/min (20 in./min.); ASTM D638, Type IV Specimen
Flexural Modulus 0.310 GPa
45.0 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525
Brittleness Temperature -58.0 °C
-72.4 °F
ASTM D746
Descriptive Properties Value Comments
Process Coating