Eagle Brass 305 Austenitic Stainless Steel, 1/2 Hardened

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Eagle Brass Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 305 Austenitic Stainless Steel, 1/2 Hardened.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type 305 is a chromium nickel stainless steel that can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is nonmagnetic under most conditions. Typical uses include appliances, kitchen utensils, tank covers and other deep drawn parts.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 7.92 g/cc
0.286 lb/in³
As Annealed
Mechanical Properties Metric English Comments
Tensile Strength >= 1030 MPa
>= 150000 psi
Tensile Strength, Yield >= 758 MPa
>= 110000 psi
0.2% Offset
Elongation at Break >= 6.0 %
>= 6.0 %
in 2 inches
Tensile Modulus 193 GPa
28000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.9 µm/m-°C

@Temperature 20.0 - 649 °C
10.5 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 15.4 W/m-K
107 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.12 %
<= 0.12 %
Chromium, Cr 17 - 19 %
17 - 19 %
Iron, Fe 65.055 - 72.5 %
65.055 - 72.5 %
Calculated as Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni 10.5 - 13 %
10.5 - 13 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.030 %
<= 0.030 %