Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AIM 58 Fusible Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer AIM Specialty Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AIM 58 Fusible Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: lens blocking; proof casting; fusible element in safety devices; anchoring parts for machining; sealing adjustment screws; holding jet engine blades for machining and broaching; filler for supporting castings in interrupted cuts.These silvery white alloys expand only ~3.3% of their volume when changing from liquid to solid form, which makes these alloys ideal for many industrial applications. AIM fusible alloys are rarely consumed in an operation and therefore can be remelted and used multiple times. These alloys are normally used in gravity casting but also can be used in other casting methods.Information provided by AIM Specialty Materials.
Physical Properties Metric English Comments
Density 8.58 g/cc
0.310 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 14
14
Tensile Strength, Ultimate 43.4 MPa
6300 psi
Elongation at Break 50 %
50 %
Thermal Properties Metric English Comments
Heat of Fusion 18.6 J/g
8.00 BTU/lb
CTE, linear 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.134 J/g-°C
0.0320 BTU/lb-°F
Liquid
0.134 J/g-°C
0.0320 BTU/lb-°F
Solid
Melting Point 58.0 °C
136 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 49 %
49 %
Indium, In 21 %
21 %
Lead, Pb 18 %
18 %
Tin, Sn 12 %
12 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000710 ohm-cm
0.0000710 ohm-cm
Copyright © lookpolymers.com All Rights Reserved