Material Notes:
32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line.
Physical Properties Metric English Comments
Moisture Absorption at Equilibrium 3.9 %
3.9 %
Equilibrium at 65% RH
3.9 %
3.9 %
65% RH
Water Absorption at Saturation 8.5 %
8.5 %
100% RH
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm
3.81 cc-mil/100 in²-24hr-atm
40°C, 90% RH
Oxygen Transmission 0.00800 cc-mm/m²-24hr-atm
0.0203 cc-mil/100 in²-24hr-atm
20°C; 65% RH; Permeability increases significantly at higher moisture content.
Thickness 15.2 microns
0.600 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 180 %
180 %
10%/min.; ASTM D638
Film Elongation at Break, TD 140 %
140 %
10%/min.; ASTM D638
Secant Modulus, MD 2.00 GPa
290 ksi
Youngs Modulus, ASTM D638, 10%/min.
Secant Modulus, TD 1.90 GPa
276 ksi
Youngs Modulus, ASTM D638, 10%/min.
Elmendorf Tear Strength MD 380 g
380 g
ASTM D638
Elmendorf Tear Strength TD 300 g
300 g
ASTM D638
Elmendorf Tear Strength, MD 24.9 g/micron
633 g/mil
0.6 mil; ASTM D638
Elmendorf Tear Strength, TD 19.7 g/micron
500 g/mil
0.6 mil; ASTM D638
Film Tensile Strength at Break, MD 80.0 MPa
11600 psi
10%/min.; ASTM D638
Film Tensile Strength at Break, TD 52.0 MPa
7540 psi
10%/min.; ASTM D638
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 20.0 °C
27.8 µin/in-°F

@Temperature 68.0 °F
Estimated by MatWeb from similar grades
110 µm/m-°C

@Temperature 100 °C
61.1 µin/in-°F

@Temperature 212 °F
Estimated by MatWeb from similar grades
Specific Heat Capacity 2.40 J/g-°C
0.574 BTU/lb-°F
Estimated by MatWeb from similar grades
Thermal Conductivity 0.340 W/m-K
2.36 BTU-in/hr-ft²-°F
For EVAL F101
Melting Point 181 °C
358 °F
DSC
Optical Properties Metric English Comments
Haze 1.5 %
1.5 %
65% RH
Gloss 90 %
90 %
65% RH
Electrical Properties Metric English Comments
Electrical Resistivity 4.70e+12 ohm-cm
4.70e+12 ohm-cm
Surface Resistance 1.90e+15 ohm
1.90e+15 ohm
Dielectric Constant 5.5
5.5
Frequency Not Specified
Dissipation Factor 0.21
0.21
Frequency Not Specified