Polymer Property : Elmendorf Tear Strength, TD = 19.7 g/micron Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength, TD 19.7 g/micron
500 g/mil
ASTM D1922
ExxonMobil Exceed™ 1023CA Tough Premium Film Resin  (discontinued **)
Exceed 1023CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1023CA resin have outstanding tensile, impact strength and puncture. These superi..
Elmendorf Tear Strength, TD 19.7 g/micron
500 g/mil
ASTM D1922A
LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion
Key Features: polypropylene random copolymer resin formulated for cast film extrusion, good optical properties, excellent slip properties, FDA acceptable, improved cold temperature impact resistance..
Elmendorf Tear Strength, TD 19.7 g/micron
500 g/mil
based on 2 mil film; ASTM D1922
LyondellBasell Alathon® L5485 High Density Polyethylene
ApplicationsALATHON L 5485 is a medium molecular weight, high density polyethylene copolymer for use in blown film applications. Typical applications include general purpose HDPE film applications ..
Elmendorf Tear Strength, TD 19.7 g/micron
500 g/mil
ASTM D1922
Chevron Phillips MarFlex® HHM TR-130 MDPE Film Resin
Medium density resin provides overall balance of tensile, impact, and tear properties in film. It is suited for merchandise, produce, and trash bags. Processing performance is excellent on high st..
Elmendorf Tear Strength, TD 19.7 g/micron
500 g/mil
ASTM D1922
Dow FLEXOMER™ ETS-9066 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ ETS-9066 NT 7 is intended for use in single of multi-layer blown-film constructions or thick sheets. Films extruded from ETS-9064 NT 7 have a high tear strength, high impact strength, an..
Elmendorf Tear Strength, TD 19.7 g/micron
500 g/mil
0.6 mil; ASTM D638
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film  (discontinued **)
32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro..