EMS-Griltech Grilamid® DN 80 Nylon 12 Monofilament

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer EMS-Griltech
Trade Name Grilamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilamid® DN 80 Nylon 12 Monofilament.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Filament Diameter 120 - 160 µm
120 - 160 µm
Mechanical Properties Metric English Comments
Elongation at Break 10 - 30 %
10 - 30 %
Tenacity 0.446 - 0.545 N/tex
5.05 - 6.17 g/denier
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
Shrinkage 11.0 - 16.0 %

@Temperature 180 °C
11.0 - 16.0 %

@Temperature 356 °F
Thermo Shrinkage
Descriptive Properties Value Comments
Heat Setting Non-Set