Hexcel® HexPly® 954-3 Curing Cyanate Resin, M60J Fiber

Category Polymer , Thermoset , Epoxy
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 954-3 Curing Cyanate Resin, M60J Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2151 MPa

@Temperature 23.0 °C
312000 psi

@Temperature 73.4 °F
Tensile Modulus 365 GPa

@Temperature 23.0 °C
52900 ksi

@Temperature 73.4 °F
Compressive Yield Strength 924 MPa

@Temperature 23.0 °C
134000 psi

@Temperature 73.4 °F
Compressive Modulus 343 GPa

@Temperature 23.0 °C
49700 ksi

@Temperature 73.4 °F
Shear Strength 78.0 MPa

@Temperature 22.0 °C
11300 psi

@Temperature 71.6 °F