ELASTO UK Dryflex® 650600 TPE, Improved Compression Set and High Temperature Resistance, 60A Hardness

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer ELASTO UK Ltd, a Hexpol company
Trade Name Dryflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ELASTO UK Dryflex® 650600 TPE, Improved Compression Set and High Temperature Resistance, 60A Hardness.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compression set and high temperature resistance.Information from Vita Thermoplastic Polymers (VTP).Vita Thermoplastic Polymers was aquired by HEXPOL and is now ELASTO
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 10.0 kg,
Temperature 190 °C
20 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength at Break 9.40 MPa
1360 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
100% Modulus 0.00150 GPa
0.218 ksi
ASTM D638
Tear Strength 26.0 kN/m
148 pli
ASTM D624
Compression Set 17 %
17 %
at 23°C, 72 hrs; ASTM D395
27 %
27 %
at 70°C, 22 hrs; ASTM D638
Descriptive Properties Value Comments
Color Natural