Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.38 MPa @Temperature 23.0 °C |
1360 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC MT224 Thermoplastic Elastomer (TPE) Versaflex™ HC MT224 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT224 has been specially formulated without the use of any plasticize.. |
|||
Tensile Strength at Break | 9.40 MPa | 1360 psi | ASTM D412 |
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation
(discontinued **) Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont. |
|||
Tensile Strength at Break | 9.40 MPa | 1360 psi | After 7 days/150°C air oven, ASTM D573 |
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation
(discontinued **) Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont. |
|||
Tensile Strength at Break | 9.40 MPa | 1360 psi | ASTM D412 |
DuPont Elvax® 40L-08 High Temperature Ignition Cable Jacket Formulation
(discontinued **) Elvax® 40L-08 high temperature ignition cable jacket.Information provided by DuPont. |
|||
Tensile Strength at Break | 9.40 MPa | 1360 psi | After 7 days/150°C air oven, ASTM D573 |
DuPont Elvax® 40L-08 High Temperature Ignition Cable Jacket Formulation
(discontinued **) Elvax® 40L-08 high temperature ignition cable jacket.Information provided by DuPont. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | 510 mm/min; ASTM D412A |
PolyOne Synprene® RT-3790 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | ASTM D638 |
LyondellBasell Microthene® G MU76000 Ethylene Vinyl Acetate Copolymer General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Tensile Strength at Break | 9.40 MPa | 1360 psi | ASTM D638 |
ELASTO UK Dryflex® 650600 TPE, Improved Compression Set and High Temperature Resistance, 60A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
Tensile Strength at Break | 9.37 MPa | 1360 psi | ASTM D1000 |
3M Scotch® 24 Electrical Shielding Tape Scotch® 24 Electrical Shielding Tape is an all-metal, open-weave, shielding braid tape in a flat, cable-like form. It is conformable due to the open-weave knit construction of two No. AWG tinned co.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Strength at Break | 9.38 MPa | 1360 psi | AVG; ASTM D412 Method A |
Seals Eastern 5861 Fluoro-silicone Fluoro-silicone meeting MIL-R-25988BInformation provided by Seals Eastern, Inc. |