Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00150 GPa | 0.218 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TP-759 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | |
Natural Rubber, Vulcanized (NR, IR, Polyisoprene) Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.Natural rubber.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TP-759 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00150 - 0.00170 GPa | 0.218 - 0.247 ksi | DIN 53504 S2 |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | ISO 37 |
ELASTO UK Dryflex® 3006-101 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3006-101 is specifically designe.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | ISO 37 |
ELASTO UK Dryflex® 3037-111 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3037-111 is specifically designe.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | ISO 37 |
ELASTO UK Dryflex® 3039-201 TPE, Modified Injection Molding Grade for Sanitary Seals The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3039-201 is specifically designe.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | ASTM D638 |
ELASTO UK Dryflex® 650600 TPE, Improved Compression Set and High Temperature Resistance, 60A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | ISO 37 |
AlphaGary Evoprene™ 003 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | ISO 37 |
AlphaGary Evoprene™ 068 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Black Peroxide Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
100% Modulus | 0.00150 - 0.00200 GPa | 0.218 - 0.290 ksi | DIN 53504 S2 |
Wacker Silicones Geniomer® 60 Silicone TPE SLM TPSE 60 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phase.. |
|||
100% Modulus | 0.00150 GPa | 0.218 ksi | ISO 37 |
AlphaGary Evoprene™ GC 5688 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |