Polymer Property : Tensile Strength at Break = 9.40 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.40 MPa
1360 psi
ASTM D412
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation  (discontinued **)
Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont.
Tensile Strength at Break 9.40 MPa
1360 psi
After 7 days/150°C air oven, ASTM D573
DuPont Elvax® 40L-03 High Temperature Ignition Cable Jacket Formulation  (discontinued **)
Elvax® 40L-03 high temperature ignition cable jacket.Information provided by DuPont.
Tensile Strength at Break 9.40 MPa
1360 psi
ASTM D412
DuPont Elvax® 40L-08 High Temperature Ignition Cable Jacket Formulation  (discontinued **)
Elvax® 40L-08 high temperature ignition cable jacket.Information provided by DuPont.
Tensile Strength at Break 9.40 MPa
1360 psi
After 7 days/150°C air oven, ASTM D573
DuPont Elvax® 40L-08 High Temperature Ignition Cable Jacket Formulation  (discontinued **)
Elvax® 40L-08 high temperature ignition cable jacket.Information provided by DuPont.
Tensile Strength at Break 9.40 MPa
1360 psi
ASTM D638
ELASTO UK Dryflex® 650600 TPE, Improved Compression Set and High Temperature Resistance, 60A Hardness
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi..