Material Notes:
Product Description: Mylar® OWF2 is a co-extruded, one side amorphous, heat sealable polyester film designed to be used as an overwrap film. Mylar® OWF2 has a thicker heat sealable layer than Mylar® OWF. This film is suitable for use in contact with food. Approvals: FDA Food Contact Status - All gauges of Mylar® OWF2 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® OWF2 can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 100 %
100 %
ASTM D882A
Film Elongation at Break, TD 90 %
90 %
ASTM D882A
Coefficient of Friction, Dynamic 0.50
0.50
A-B; ASTM D1894
Coefficient of Friction, Static 0.60
0.60
ASTM D1894
Film Tensile Strength at Break, MD 172 MPa
25000 psi
ASTM D882A
Film Tensile Strength at Break, TD 186 MPa
27000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Maximum Service Temperature, Air 121 °C
250 °F
Shrinkage, MD 1.25 %

@Temperature 150 °C,
Time 1800 sec
1.25 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.30 %

@Temperature 150 °C,
Time 1800 sec
0.30 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 3.5 %
3.5 %
ASTM D1003
Transmission, Visible 88.6 %
88.6 %
ASTM D1003
Descriptive Properties Value Comments
Gas Permeability (Base film) 5 cc/100 in2
O2, 24 hr; ASTM D3985 77°F/75% RH/1 ATM
Yield (nominal) 33000 in2/lb