Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Mylar® EB11 Polyester Film, 92 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® EB11 Polyester Film, 92 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mylar® EB11 is a low gloss polyester film with a matte surface. It is typically used as a carrier film. It is commercially available in nominal 48 - 300 gauge. General Product Info: Mylar® EB11 is a low gloss, hazy product. Reverse side printing is good, and metallized EB11 offers muted matte appearance. EB11 provides an excellent, low gloss surface texture transfer when used as a carrier film.Approvals: FDA Food Contact Status - All gauges of Mylar® EB11 comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers, Sections (f), (g), and (h). This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® EB11 can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 144 %
144 %
ASTM D882A
Film Tensile Strength at Break, MD 131 MPa
19000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Maximum Service Temperature, Air 121 °C
250 °F
Shrinkage, MD 1.5 %

@Temperature 150 °C,
Time 1800 sec
1.5 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.0 %

@Temperature 150 °C,
Time 1800 sec
1.0 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 60 %
60 %
ASTM D1003
Gloss 46 %
46 %
60°; ASTM D2457 - 90
Transmission, Visible 83 %
83 %
TLT; ASTM D1003
Users viewing this material also viewed the following: