Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Mylar® E Polyester Film, 92 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Mylar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Mylar® E Polyester Film, 92 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mylar® E polyester film is a clear smooth base film engineered to provide superior optical and physical properties required of critical dying, metallizing, laminating, labeling and coating applications while processing excellent winding and handling characteristics. General Product Info: Mylar® E polyester film combines the optical properties of low haze, high clarity in a base film with the surface characteristics need for high speed converting and winding without the effect of grainy haze. Its physical strength and dimensional stability are ideally suited for both converting ease and end-use performance.Typical Applications: Mylar® E polyester film is particularly suitable for use in solar film applications as well as other critical applications requiring the unique balance of superior optical and excellent handling characteristics.Approvals: FDA Food Contact Status - All gauges of Mylar® E comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® E can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F. UL 94 VTM-2 - for 92 gauge (0.13mm) only.Information provided by DuPont.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Typical Mylar®; ASTM D1505
Mechanical Properties Metric English Comments
Film Elongation at Break, MD >= 75 %
>= 75 %
ASTM D882A
Film Elongation at Break, TD >= 55 %
>= 55 %
ASTM D882A
Film Tensile Strength at Break, MD 172 MPa
25000 psi
ASTM D882A
Film Tensile Strength at Break, TD 186 MPa
27000 psi
ASTM D882A
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C
0.280 BTU/lb-°F
Typical Mylar®
Melting Point 254 °C
489 °F
Typical Mylar® via DSC
Maximum Service Temperature, Air 121 °C
250 °F
Shrinkage, MD 1.9 %

@Temperature 150 °C,
Time 1800 sec
1.9 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.4 %

@Temperature 150 °C,
Time 1800 sec
1.4 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Refractive Index 1.64 - 1.67
1.64 - 1.67
typical of Mylar®
Haze 2.1 %
2.1 %
ASTM D1003
Descriptive Properties Value Comments
Wyco Ra 11 nm
M930.8500
Yield (nominal) 21500 in2/lb
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved