Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® ST557 Polyester Film, 200 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® ST557 Polyester Film, 200 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® ST557 is a slightly hazy polyester film with low shrinkage, good flatness, and excellent handling properties. Melinex® ST557 is pretreated with a unique primer on both surfaces for adhesion in special applicationsInformation provided by DuPont.
Mechanical Properties Metric English Comments
Coefficient of Friction, Static <= 0.50
<= 0.50
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 50.0 °C
10.0 µin/in-°F

@Temperature 68.0 - 122 °F
Melting Point 265 °C
509 °F
Shrinkage, MD 0.15 %

@Temperature 150 °C,
Time 1800 sec
0.15 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.15 %

@Temperature 150 °C,
Time 1800 sec
0.15 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Transmission, Visible 85.5 %
85.5 %
TLT; ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistivity per Square 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
Dielectric Constant 2.9

@Frequency 100 Hz
2.9

@Frequency 100 Hz
ASTM D150
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149
Dielectric Breakdown 10000 V
10000 V
ASTM D149
Descriptive Properties Value Comments
Coefficient of Hygroscopic Expansion 0.000008 IN/IN/% RH
40% - 80% RH
Flexural Strength >20000 cycles
ASTM D2176
Users viewing this material also viewed the following: