Polymer Property : Dielectric Strength = 197 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149-09
NeXolve LaRC™-CP1 Polyimide
Transparent polyimide with low moisture uptake and low dielectric constant. Transparent polyimide with low moisture uptake and low dielectric constant. LaRC™ CP1 exhibits the lowest moisture uptak..
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149(A)
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film  (discontinued **)
Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc..
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D-149
Saint-Gobain Norton® PMP Film
Features/Benefits:Good release properties for up to 180°C (356°F) cure composites (application dependent)low density for high surface area per poundExcellent clarityThermoformableProduct avail..
Dielectric Strength 197 kV/mm
5000 kV/in
DuPont™ Kapton® 150FN019 Polyimide/FEP Composite Film
150 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r..
Dielectric Strength 197 kV/mm
5000 kV/in
DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film
250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r..
Dielectric Strength 197 kV/mm
5000 kV/in
Flat sheets in air placed between 1/4 in diameter brass electrodes with 0.8 mm (1/32 in) edge radius subjected to 60 cycles AC voltage at 600V/s rate of rise to the breakdown voltage.; ASTM D149-81
DuPont™ Kapton® 300A Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)Kapton® Type A is a lower modulus film, which is conducive to dynamic flex applications.General Kapton® information: Kapton® is synthesized by polymerizing an a..
Dielectric Strength 197 kV/mm
5000 kV/in
Flat sheets in air placed between 1/4 in diameter brass electrodes with 0.8 mm (1/32 in) edge radius subjected to 60 cycles AC voltage at 600V/s rate of rise to the breakdown voltage.; ASTM D149-81
DuPont™ Kapton® 300FPC Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick..
Dielectric Strength 197 kV/mm
5000 kV/in
Flat sheets in air placed between 1/4 in diameter brass electrodes with 0.8 mm (1/32 in) edge radius subjected to 60 cycles AC voltage at 600V/s rate of rise to the breakdown voltage.; ASTM D149-81
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Dielectric Strength 197 kV/mm
5000 kV/in
Flat sheets in air placed between 1/4 in diameter brass electrodes with 0.8 mm (1/32 in) edge radius subjected to 60 cycles AC voltage at 600V/s rate of rise to the breakdown voltage.; ASTM D149-81
DuPont™ Kapton® 300KN Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dian..
Dielectric Strength 197 kV/mm
5000 kV/in
Flat sheets in air placed between 1/4 in diameter brass electrodes with 0.8 mm (1/32 in) edge radius subjected to 60 cycles AC voltage at 600V/s rate of rise to the breakdown voltage.; ASTM D149-81
DuPont™ Kapton® 300VN Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type HN with added dimensional stability. Available i..
Dielectric Strength 197 kV/mm
5000 kV/in
Flat sheets in air placed between 1/4 in diameter brass electrodes with 0.8 mm (1/32 in) edge radius subjected to 60 cycles AC voltage at 600V/s rate of rise to the breakdown voltage.; ASTM D149-81
DuPont™ Kapton® 300ZT Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN and HN with superior bondability. Available i..
Dielectric Strength 197 kV/mm
5000 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Melinex® 329 Polyester Film, 92 Gauge
Melinex® 329 is an opaque white, non-pretreated, polyester film with good handling properties and a unique glossy appearance. It is used as a base for pressure sensitive labels, in security and ac..
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149
DuPont Teijin Films Melinex® 329S Polyester Film, 92 Gauge
An opaque white film with good handling properties, a unique glossy appearance, and a lower shrinkage for special applicationsInformation provided by DuPont.
Dielectric Strength 197 kV/mm
5000 kV/in
0.25 inch electrodes in dry air @25°C; ASTM D149-81
DuPont Teijin Films Melinex® S Polyester Film, 200 Gauge
Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for ..
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST579 Polyester Film, 200 Gauge
Melinex® ST579 is a clear, heat stabilized polyester film that is primed on one surface for adhesion. Typical applications include flexible electronics, touch screens, displays, circuitry, and othe..
Dielectric Strength 197 kV/mm
5000 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Melinex® SWC Polyester Film, 200 Gauge
A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi..
Dielectric Strength 197 kV/mm
5000 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Melinex® XST6562 Polyester Film, 200 Gauge
Melinex® XST6562 is a thermally stabilized high clarity polyester film with good handleability. It is pretreated on one film surface to promote adhesion.Information provided by DuPont.
Dielectric Strength 197 kV/mm
5000 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Melinex® 6428 Polyester Film, 200 Gauge
Melinex® 6428 is a high clarity polyester film. It is pretreated on both film surfaces to promote adhesion to EVA. Melinex® 6428 is a developmental film designed for the photovoltaics industry.Als..
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST580 Polyester Film, 200 Gauge
Melinex® ST580 is a clear, heat stabilized polyester film that is primed on one surface for enhanced adhesion to UV curable inks and coatings. Typical applications include flexible electronics, tou..
Dielectric Strength 197 kV/mm
5000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST557 Polyester Film, 200 Gauge
Melinex® ST557 is a slightly hazy polyester film with low shrinkage, good flatness, and excellent handling properties. Melinex® ST557 is pretreated with a unique primer on both surfaces for adhesi..
Dielectric Strength 197 kV/mm
5000 kV/in
Value for a 1 mil sample.; ASTM D-149
Saint-Gobain Norton® MFA Fluoropolymer Film
Features/Benefits:Outstanding clarityPerformance from -254°C (-425°F) to 230°C (446°F)Outstanding flex life and stress-crack resistanceOutstanding anti-stick release propertiesExcellent electric..