Polymer Property : Tensile Strength = 52.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 52.0 MPa
7540 psi
Nihon Superior SN100CL Lead-Free Solder Alloy
Used for hot air solder leveling (HASL). Features include: Excellent fluidity; Bridge-free coating of the fine pitch circuitry; Bright smooth and uniform coating; Low copper erosion; Formation of st..
Tensile Strength 52.0 MPa
7540 psi
ISO 527
Lucite International Diakon® Frost 902 70 Acrylic Polymer
Information provided by Lucite International
Tensile Strength 52.0 MPa
7540 psi
ISO 527
Lucite International Diakon® TD625 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Tensile Strength 52.0 MPa
7540 psi
ASTM D638
Samyang Trimma® SD6310H PMMA, Translucent
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat..
Tensile Strength 52.0 MPa
7540 psi
DAM; ASTM D638
DuPont Performance Polymers Elvamide® 8063 Nylon  (Unverified Data**)
Polyamide Multipolymer with Improved Gel Resistance in SolutionsInformation provided by DuPont Performance Polymers
Tensile Strength 52.0 MPa
7540 psi
DIN 53 455
Hippe PBT Polybutylene Terephthalate
The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe.
Tensile Strength >= 52.0 MPa
>= 7540 psi
ISO 37
Austin Novel Materials Texalan® 372D Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Strength >= 52.0 MPa
>= 7540 psi
ISO 37
Austin Novel Materials Texalan® 464D Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Strength >= 52.0 MPa
>= 7540 psi
ISO 37
Austin Novel Materials Texalan® 564D Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Strength >= 52.0 MPa
>= 7540 psi
ISO 37
Austin Novel Materials Texalan® 772D PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Strength >= 52.0 MPa
>= 7540 psi
ISO 37
Austin Novel Materials Texalan® 672D Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Strength 52.0 MPa
7540 psi
5 mm/min; ISO 527-1
Sax Polymers SAXALEN PPH121GK30 Polypropylene Homopolymer, 30% Glass Filled
SAXALEN PPH121GK30 is a 20% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. This type has a higher stiffness and a optimized warpage grade.Informat..
Tensile Strength 52.0 MPa
7540 psi
ISO 527
Lucite International Diakon® Frost 902 80 Acrylic Polymer
Information provided by Lucite International