Dow SPECFLEX™ NC 700 Polyol

Category Polymer
Manufacturer Dow Chemical
Trade Name SPECFLEX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow SPECFLEX™ NC 700 Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SPECFLEX™ NC 700 polyol is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile. It is manufactured without the use of BHT and has been filtered to 200 microns. CAS# 009082-00-2 057913-80-1Information provided by Dow
Physical Properties Metric English Comments
Specific Gravity 1.049 g/cc
1.049 g/cc
Solids Content 39 - 42 %
39 - 42 %
Viscosity 310 cP

@Temperature 98.9 °C
310 cP

@Temperature 210 °F
2360 cP

@Temperature 37.8 °C
2360 cP

@Temperature 100 °F
4810 cP

@Temperature 25.0 °C
4810 cP

@Temperature 77.0 °F
28530 cP

@Temperature 0.000 °C
28530 cP

@Temperature 32.0 °F
Maximum Moisture Content 0.070
0.070
wt% water
Vapor Pressure <= 0.0000133 bar
<= 0.0100 torr
Thermal Properties Metric English Comments
Specific Heat Capacity 1.57 J/g-°C

@Temperature 20.0 °C
0.375 BTU/lb-°F

@Temperature 68.0 °F
1.72 J/g-°C

@Temperature 60.0 °C
0.411 BTU/lb-°F

@Temperature 140 °F
2.03 J/g-°C

@Temperature 100 °C
0.485 BTU/lb-°F

@Temperature 212 °F
Thermal Conductivity 0.166 W/m-K
1.15 BTU-in/hr-ft²-°F
0.164 W/m-K

@Temperature 100 °C
1.14 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.165 W/m-K

@Temperature 50.0 °C
1.14 BTU-in/hr-ft²-°F

@Temperature 122 °F
Flash Point >= 169 °C
>= 336 °F
Descriptive Properties Value Comments
Hydroxyl Number mg KOH/g 19.5 - 23
Users viewing this material also viewed the following: