Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.57 J/g-°C @Temperature 20.0 °C |
0.375 BTU/lb-°F @Temperature 68.0 °F |
|
Dow SPECFLEX™ NC 700 Polyol SPECFLEX™ NC 700 polyol is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile. It is manufactured without the use of BHT and has been filtered to 200 microns. CA.. |