Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 28530 cP @Temperature 0.000 °C |
28530 cP @Temperature 32.0 °F |
|
Dow SPECFLEX™ NC 700 Polyol SPECFLEX™ NC 700 polyol is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile. It is manufactured without the use of BHT and has been filtered to 200 microns. CA.. |