Dow GRSN-2070 NT Linear Low Density Polyethylene Granular Solid

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Dow Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow GRSN-2070 NT Linear Low Density Polyethylene Granular Solid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW GRSN-2070 NT is produced using UNIPOL™ process technology. It is granular product intended for use in the production of color concentrates and master batches. Information provided by Dow
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
natural resin; ASTM D792
High Load Melt Index 52 g/10 min

@Load 21.6 kg,
Temperature 190 °C
52 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Melt Index of Compound 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 121 °C
250 °F
Dow Method (DSC)