LG Chemical IM812 Acrylic impact modifier

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical IM812 Acrylic impact modifier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: LG AIM (Acrylic impact modifier) is a type of additives that improves weather-resistance, impact strength, and processability of thermoplastic resin including PVC, which is used for products of outdoor applications.Application: Sheet, Pipe, Fitting etcInformation provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.02 - 1.20 g/cc
1.02 - 1.20 g/cc
Bulk Density >= 0.390 g/cc
>= 0.0141 lb/in³
Aerated; LSY-QB-KD019
Volatiles <= 1.0 %
<= 1.0 %
ISO 1625
Particle Mesh Size 20 Mesh
20 Mesh
<3%, (mesh on); LSY-QB-KD022
200 Mesh
200 Mesh
<20%, (mesh pass); LSY-QB-KD023
Vapor Pressure 0.0227 bar

@Temperature 20.0 °C
17.0 torr

@Temperature 68.0 °F
Thermal Properties Metric English Comments
Melting Point 132 - 149 °C
270 - 300 °F
Flash Point 400 °C
752 °F
Descriptive Properties Value Comments
Caking <90%
LSY-QB-KD009
Foreign Material <3 (10 x 10 cm)
LSY-QB-KD005
Fusion time 35-60 sec
ISO 1830-6