Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning SILASTIC® V RTV SILICONE RUBBER BASE & CURING AGENT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® V RTV SILICONE RUBBER BASE & CURING AGENT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength silicone rubber featuring medium durometer, low mixed viscosity, suited for the reproduction of architectural, furniture components and prototypes. Silastic V is recommended for use with rigid and foam polyurethane and can be used with polyester, cement and plaster.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc

@Temperature 25.0 °C
1.35 g/cc

@Temperature 77.0 °F
Viscosity 38300 cP
38300 cP
mixing, dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
Tensile Strength, Ultimate 6.27 MPa
910 psi
Elongation at Break 500 %
500 %
Tear Strength 31.6 kN/m
180 pli
Descriptive Properties Value Comments
Approximate De-mold Time (hours) 6-8
Color purple
Mix Ratio (X:1) 10
Base to Catalyst
Working Time (min) 60-90
Users viewing this material also viewed the following: