Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 38300 cP | 38300 cP | mixing, dynamic |
Dow Corning SILASTIC® V RTV SILICONE RUBBER BASE & CURING AGENT High strength silicone rubber featuring medium durometer, low mixed viscosity, suited for the reproduction of architectural, furniture components and prototypes. Silastic V is recommended for use wi.. |