Dow Corning SILASTIC® P-1 RTV SILICONE RUBBER & CLEAR CURING AGENT

Category Polymer , Adhesive , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® P-1 RTV SILICONE RUBBER & CLEAR CURING AGENT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High strength silicone rubber suited for prototyping, production tooling, artistic and renovation applications. Silastic P-1 is recommended for use with polyesters, cement and rigid polyurethanes; also can be used with plaster.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc

@Temperature 25.0 °C
1.12 g/cc

@Temperature 77.0 °F
Viscosity 13500 cP
13500 cP
mixing, dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
Tensile Strength, Ultimate 7.45 MPa
1080 psi
Elongation at Break 850 %
850 %
Tear Strength 22.8 kN/m
130 pli
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Descriptive Properties Value Comments
Appearance clear
curing agent
Color off-white
Mix Ratio (X:1) 10
Base to Catalyst
Working Time (min) 45