CMW® ELKONIUM 305 platinum based alloy

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer CMW Inc.
Trade Name ELKONIUM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONIUM 305 platinum based alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (1769(C) and good resistance to forming arcs. Low electrical conductivity (15% IACS) limits its application to low currents, usually below 5 amperes. Because of the high cost of the platinum ELKONIUM alloys, they are almost always supplied as composite contacts with thin facings of the ELKONIUM metal (silver brazed to nickel plated steel backings in the form of rivets, screws and weld buttons).ELKONIUM 34, ELKONIUM 305 and ELKONIUM 306 alloys have lower ruthenium contents and are softer and more ductile. They can be headed into rivets over a limited range. All five alloys have low transfer characteristics and are used in voltage regulators and motor speed governors. They can be used as a positive contact paired with tungsten negative contact for improved transfer resistance. They also have high tarnish resistance and are suitable for many sensitive, low voltage applications.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 20.6 g/cc
0.744 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 84
84
annealed
89
89
cold worked
Tensile Strength, Ultimate 414 MPa
60000 psi
annealed
793 MPa
115000 psi
cold worked
Elongation at Break 5.0 %
5.0 %
cold worked
18 %
18 %
annealed
Component Elements Properties Metric English Comments
Platinum, Pt 95 %
95 %
Ruthenium, Ru 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000344 ohm-cm
0.0000344 ohm-cm
5 % IACS