Schott S8008G Contrast Enhancement Filter

Category Ceramic , Glass , Filter
Manufacturer Schott North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott S8008G Contrast Enhancement Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 2.74 g/cc
0.0990 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.90 µm/m-°C

@Temperature 20.0 - 300 °C
4.94 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 487 °C
909 °F
Softening Point 671 °C
1240 °F
Working Point 909 °C
1670 °F
Annealing Point 503 °C
937 °F
Strain Point 475 °C
887 °F
Optical Properties Metric English Comments
Refractive Index 1.548
1.548
n<sub>d</sub>, Sodium
Descriptive Properties Value Comments
Color Green
Half Bandwidth (nm) <28
Transmission at Peak (%) 10.5-12.5
Wavelength of Maximum Transmission (nm) 542-546