Diapolyacrylate Shinko-Lac® U400B Transparent ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer Diapolyacrylate Company Limited
Trade Name Shinko-Lac®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diapolyacrylate Shinko-Lac® U400B Transparent ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Shinko-Lac® is a registered trademark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Melt Flow 0.30 g/10 min

@Load 5.00 kg,
Temperature 220 °C
0.30 g/10 min

@Load 11.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength at Break 41.0 MPa
5950 psi
ASTM D638
Flexural Yield Strength 66.0 MPa

@Thickness 6.35 mm
9570 psi

@Thickness 0.250 in
ASTM D790
Flexural Modulus 1.90 GPa

@Thickness 6.35 mm
276 ksi

@Thickness 0.250 in
ASTM D790
Izod Impact, Notched 0.998 J/cm

@Thickness 6.40 mm
1.87 ft-lb/in

@Thickness 0.252 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 100 °C
212 °F
ISO R-306; 49N
Optical Properties Metric English Comments
Transmission, Visible 90 %

@Thickness 3.20 mm
90 %

@Thickness 0.126 in
ASTM D1003