Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP25-1503 GF25 25% Glass Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 20% Glass Fiber Filler , Polypropylene with 30% Glass Fiber Filler
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-1503 GF25 25% Glass Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Melt Flow 14.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.0 MPa
8850 psi
chs 0.2 in/min; ASTM D638
Elongation at Yield 9.4 %
9.4 %
chs 0.2 in/min; ASTM D638
Flexural Strength 94.0 MPa
13600 psi
ASTM D790
Flexural Modulus 3.918 GPa
568.3 ksi
ASTM D790
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm
3.001 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
0.125";; ASTM D648
Descriptive Properties Value Comments
Glass Content (%) 25
ASTM D2584
Copyright © lookpolymers.com All Rights Reserved