Polymer Property : Flexural Modulus = 3.918 GPa
Polymer Property :
Flexural Modulus =
3.918 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
3.918
GPa
568.3
ksi
ASTM D790
Diamond Polymers NPP25-1503 GF25 25% Glass Filled Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.