Mechanical Properties Metric English Comments
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.001 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Lucent Polymers 66-41 Nylon 66, Toughened
Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.001 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Lucent Polymers ABS-305 Acrylonitrile Butadiene Styrene, General Purpose
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.001 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Lucent Polymers ABS-305LG Acrylonitrile Butadiene Styrene, General Purpose, Low Gloss
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.001 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Lucent Polymers GPCB-330 Polycarbonate+PBT, 30% Glass Fiber Reinforced, Impact Resistant
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm
3.001 ft-lb/in

@Thickness 0.125 in
ASTM D256
Lucent Polymers GPP-320 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm
3.001 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm
3.001 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers NPP25-1111 CF15 Conductive Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 1.602 J/cm

@Thickness 3.17 mm
3.001 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers NPP25-1503 GF25 25% Glass Filled Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.