Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers NPP25-0504LGF40 40% Long Glass Fiber Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene with 40% Glass Fiber Filler
Manufacturer Diamond and Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP25-0504LGF40 40% Long Glass Fiber Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
chs 2.0 in/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
chs 2.0 in/min; ASTM D638
Flexural Modulus 7.584 GPa
1100 ksi
chs 0.05 in/min; tangent; ASTM D790
Izod Impact, Notched 2.25 J/cm

@Thickness 3.17 mm
4.22 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
0.125";; ASTM D648
Descriptive Properties Value Comments
Glass Content (%) 40
ASTM D2584