Diamond Polymers NPP11-0218 Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Diamond and Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers NPP11-0218 Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.1 MPa

@Thickness 0.0200 mm
3500 psi

@Thickness 0.000787 in
Transverse to Flow; ASTM D882
29.6 MPa

@Thickness 0.0200 mm
4290 psi

@Thickness 0.000787 in
Direction of Flow; ASTM D882
Elongation at Break 750 %

@Thickness 0.0200 mm
750 %

@Thickness 0.000787 in
Transverse to Flow; ASTM D882
800 %

@Thickness 0.0200 mm
800 %

@Thickness 0.000787 in
Direction of Flow; ASTM D882
Dart Drop, Total Energy 130 J
95.9 ft-lb
F50; ASTM D1709
Tear Strength Test 350

@Thickness 0.0200 mm
350

@Thickness 0.000787 in
g; Direction of Flow; ASTM D1922
350

@Thickness 0.0200 mm
350

@Thickness 0.000787 in
g; Transverse to Flow; ASTM D1922