Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Denka VINYKON W4203 PVC, W grade for equipment cords, for heat resistance.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
JIS-Z-8807
Deformation 8.0 %
8.0 %
JIS-K-6723
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
JIS-K-6301
Tensile Strength at Break 21.09 MPa
3059 psi
JIS-K-6723
Elongation at Break 290 %
290 %
JIS-K-6723
100% Modulus 0.0151 GPa
2.19 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -17.0 °C
1.40 °F
JIS-K-6723
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+13 ohm-cm
<br>@Temperature 60.0 °C
8.00e+13 ohm-cm
<br>@Temperature 140 °F
JIS-K-6723
6.00e+14 ohm-cm
<br>@Temperature 30.0 °C
6.00e+14 ohm-cm
<br>@Temperature 86.0 °F
JIS-K-6723
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 98
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 98
JIS-A-5756
Oil Resistance: Retention of Tensile Strength, % 93
JIS-K-6723
Oil Resistance: Retention Rate of Elongation, % 88
JIS-K-6723
Thermostability, min, JIS-K-6723 >240