Denka VINYKON S3098 PVC, S grade for refrigerator gaskets

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON S3098 PVC, S grade for refrigerator gaskets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
JIS-Z-8807
Evaporation Loss 0.30 %
0.30 %
JIS-A-5756
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
JIS-K-6301
Tensile Strength at Break 15.21 MPa
2205 psi
JIS-K-6723
Elongation at Break 370 %
370 %
JIS-K-6723
100% Modulus 0.0063765 GPa
0.92485 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Softening Point -24.0 °C
-11.2 °F
JIS-A-5756
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 97
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 98
JIS-A-5756