Thermal Properties Metric English Comments
Softening Point -24.0 °C
-11.2 °F
JIS-A-5756
Denka VINYKON S3098 PVC, S grade for refrigerator gaskets
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..