Denka VINYKON S3029 PVC, S grade for window frame gaskets

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Denka
Trade Name VINYKON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Denka VINYKON S3029 PVC, S grade for window frame gaskets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding, etc.
Physical Properties Metric English Comments
Density 1.345 g/cc
0.04859 lb/in³
JIS-Z-8807
Evaporation Loss 4.2 %
4.2 %
JIS-A-5756
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
JIS-K-6301
Tensile Strength at Break 12.26 MPa
1779 psi
JIS-A-5756
Elongation at Break 395 %
395 %
JIS-K-5756
100% Modulus 0.0041202 GPa
0.59759 ksi
JIS-A-5756
Thermal Properties Metric English Comments
Softening Point -46.0 °C
-50.8 °F
JIS-A-5756
Descriptive Properties Value Comments
Heating: Retention Rate of Elongation, % 88
JIS-A-5756
Heating: Retention Rate of Tensile Strength, % 104
JIS-A-5756