Polymer Property : Softening Point = -50.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Softening Point -46.0 °C
-50.8 °F
JIS-A-5756
Denka VINYKON S3029 PVC, S grade for window frame gaskets
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Softening Point -46.0 °C
-50.8 °F
JIS-A-5756
Denka VINYKON S3029A PVC, S grade for window frame gaskets
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..
Softening Point -46.0 °C
-50.8 °F
JIS-A-5756
Denka VINYKON TS1007T PVC, S grade for window frame gaskets
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..