Polymer Property : Density = 1.345 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.345 g/cc
0.04859 lb/in³
ISO 1183
Lanxess Durethan® BKV 20 FN00 000000 Nylon 6, 18% Glass Fiber
PA6, injection molding grade, 18% glass fibers, UL94 V-0 at 0,75 mm ( in house test), free of halogen and red phosphorus, specially for electro/electronic applications in regard to IEC60335-1
Density 1.345 g/cc
0.04859 lb/in³
JIS-Z-8807
Denka VINYKON S3029 PVC, S grade for window frame gaskets
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..